Home | 中文版 | sitemap  
Property
Value
Unit
Testing
Specific gravity
0.95±0.03
g/cm
ASTM D792
Hardness
45±3
Shore D
ASTM D2240
Tensile strength
110
Kg/cm
ASTM D412
Elongation
300
%
ASTM D412
Tear resistance
17
Kg/cm
ASTM D624 Die C
Heat aging resistance
100/105
% TB/EB
ASTM D573 136°C 7D
Yerzley resilitence
65
%
CNC K1392
Heater resistance
90/95
% TB/EB
W-O-M 63°C 500hrs
Brittle temperature
-60
% TB/EB
ASTM D746
Remarks Suggestion of temperature : 170°C~200°C
Test item
Specification standard
Test result
Hardness CNS 3555 typea 60°±3
Tensile strength CNS 3553 30±5%
Elongation CNS 3553 250±5%
Tear strength CNS 3559 20±5%
Specific gravity CNS 5341 1
Akron abrasion CNS 734 0.4±5%
Test item
Specification standard
Test result
Hardness CNS 3555 typea 60°±3
Tensile strength CNS 3553 50±5%
Elongation CNS 3553 350±5%
Tear strength CNS 3559 25±5%
Specific gravity CNS 5341 0.95
Akron abrasion CNS 734 0.3±5%
Test item
Specification standard
Test result
Hardness CNS 3555 typea 40°~50°
Tensile strength CNS 3553 15±2 kgf/cm2
Elongation CNS 3553 330%
Tear strength CNS 3559 15 kgf/cm
Specific gravity CNS 5341 1%
Akron abrasion CNS 734 0.5%
Test item
Specification standard
Test result
Hardness CNS 3555 typea 60°±3
Tensile strength CNS 3553 25±5% kgf/cm
Elongation CNS 3553 205±5%
Tear strength CNS 3559 20±5% kgf/cm
Specific gravity CNS 5341 1.0±5%
Akron abrasion CNS 734 0.4±5%
Test item
Specification standard
Test result
Hardness CNS 3555 typea 60°±3
Tensile strength CNS 3553 30±5%
Elongation CNS 3553 250±5%
Tear strength CNS 3559 20±5%
包裝: N.W: 25kg/bag G.W: 25.2/bags   整櫃: 17,000 kgs/container