Home | 中文版 | sitemap  
Property
Value
Unit
Testing
Density
200~220
Kg/m3
ASTM-D-3575
Hardness
58~60
(Shore A)
ASTM-D-2240
Tensile strength at break
22~28
Kg/cm2
ASTM-D-412
Elongation of break
230~250
%
500 mm/min
Split tear
3~3.5
Kg/cm
ASTM-D-3574
Compression set 50C/6h
45~50
%
ASTM-D-395
Synamic compression set
11~13
%
Resiliency
35
%
ASTM-D-2632
Mould release
good
 
Skin quality smooth    
Stations temperature: 178~188 c
Speed steps for injections: 20~30 max flow %(due to mould size)
Injection pressure: 80~90 bar (Due to mould size)
Cyele time 400~480 sec.(Due to mould size)
Expansion ratio: 1.65
Close time of mould: 0~5 sec.
Open time of mould: 5~20 sec.
Test item
Specification standard
Test result
Hardness ASTM D-2240 65°±3°
Tensile strength ASTM D-412 20~25 kgf/cm2
Elongation ASTM D-412 300 %
Tear strength ASTM D-624 15 kgf/cm2
Specific gravity ASTM D-297 0.2~0.25 g/cc
Compression set ASTM D-395 60 %
Akron abrasion CNS 734 6LB 3000 cyclex 15 angle 0.3 c.c
Test item
Specification standard
Test result
Hardness ASTM D-2240 55°±5°
Tensile strength ASTM D-412 18±5% kgf/cm2
Elongation ASTM D-412 320±5%
Tear strength ASTM D-624 9±5% kgf/cm2
Specific gravity ASTM D-297 0.2~0.23 g/cc
Compression set ASTM D-395 60±5 %
Test item
Specification standard
Test result
Hardness ASTM D-2240 50~60±3
Tensile strength ASTM D-412 16~20±5% kgf/cm
Elongation ASTM D-412 250~330±5%
Tear strength ASTM D-624 10±5% kgf/cm
Specific gravity ASTM D-297 0.22±5% g/cm
Compression set ASTM D-395 50~55±5 %
Test item
Specification standard
Test result
Hardness ASTM D-2240 55±2
Tensile strength ASTM D-412 22 (with skin)
Elongation ASTM D-412 270%
Tear strength ASTM D-624 10 kg/cm
Specific gravity ASTM D-297 0.22 g/cc
Compression set ASTM D-395 skin: 55~60 %
DETERMINATION OR COMMENTS:
1.This material maily using in slipper & mid-sole.
2.For slipper the hardness popular using in hardness 55±2 shore.
3.Slipper, Sandal, Boots and mid-sole & out-sole  of sportting shoe.